Hot vulcanization bonding method of silica gel and aluminum alloy and matters needing attention
Today not to talk about other, on the hot vulcanization of silica gel and aluminum alloy bonding method!
Aluminum alloy life is very common, a lot of doors and Windows are used aluminum alloy, in a lot of applications need and silica gel (the surface is very inert) material bonding, ordinary instant glue, quick dry glue effect is very bad, using hot vulcanized glue is a lot of people's choice, and is the right choice.
Hot vulcanization bonding method of silica gel and aluminum alloy:
Aluminum alloy belongs to the metal category, silicone and metal vulcanization molding generally use conrestate cl-26ab this glue, we use him to illustrate it!
In order to bond the good effect, the steps are also very important.
1, the first is to check the surface of the aluminum alloy has no other stains, if there is a great impact on the molding effect, need to use alcohol or toluene timely cleaning.
2. After the glue is configured in a good proportion, evenly apply it on the aluminum alloy;
3. It will take at least 30 minutes to dry at room temperature.
4. Hot vulcanized silica gel aluminum alloy is molded and bonded in the machine.
Notes for hot vulcanization bonding of silica gel and aluminum alloy:
1, in advance of the substrate corona or flame treatment can be very good to enhance the bonding effect;
2. Do not close the window or door tightly when working, and keep it ventilated.
- Store in a dry environment.